National LinerTechnical and Product Design Information - ASTM Standard
Fitting Your NeedsCertified Installers & Service ProvidersOur ProductsWho We ServeContact Us

CIPP < Product Design Information < ASTM Standard

ASTM Standard

National Liner meets or exceeds the following ASTM standards for cured-in-place pipeline rehabilitation.

F 1216
Standard practice for rehabilitation of existing pipelines and conduits by the inversion and curing of a resin impregnated tube.

D 790
Standard test methods flexural properties of unreinforced and reinforced plastics and electrical insulating materials.
  • Flexural modulus of elasticity exceeds 250,000 psi
  • Flexural strength exceeds 4,500 psi
D 638
Standard test method for tensile properties of plastics.
  • Tensile strength exceeds 3,000 psi
For the complete ASTM designation, please contact:

The American Society for Testing and Materials
100 Barr Harbor Drive
West Conshohocken, PA 19428