National Liner meets or exceeds the following ASTM standards for cured-in-place pipeline rehabilitation.
F 1216-09
Standard practice for rehabilitation of existing pipelines and conduits by the inversion and curing of a resin impregnated tube. Active Standard (Latest Version).
D 790-10
Standard test methods flexural properties of unreinforced and reinforced plastics and electrical insulating materials. Active Standard (Latest Version).
- Flexural modulus of elasticity exceeds 250,000 psi
- Flexural strength exceeds 4,500 psi
D 638-10
Standard test method for tensile properties of plastics. Active Standard (Latest Version).
- Tensile strength exceeds 3,000 psi
For the complete ASTM designation, please contact:
The American Society for Testing and Materials
100 Barr Harbor Drive
West Conshohocken, PA 19428